A new material for hip prosthesis without considerable debris release.

Adelina Borruto

Journal: Medical engineering & physics 2011;32(8):908-13

PMID: 20643571

Abstract

This work presents an alternative bearing surface in the field of total hip replacements. It is composed of a polymer composite polyether-ether-ketone (Peek) as the matrix and a carbon fibre as reinforcement. The authors carried out experimental research in order to investigate the formation of debris caused by tribological coupling of three types of Peek and cobalt chrome alloy. The wear tests (ASTM 99G) have been performed with a pin on disc tribometer in an air environment, under the following conditions: dry, water lubrication using demineralised water as a lubricant and human serum. A method of filtering under vacuum is used to extract the debris from the lubricants used in the tribological test, and the analysis at Scanning Electron Microscopy (SEM) is used to characterize the debris.

Copyright © 2010 IPEM. Published by Elsevier Ltd. All rights reserved.

Address: University of Rome La Sapienza, Department of Chemical Engineering and Materials, Via Eudossiana, 18, 00184 Rome, Italy. [email protected]
Bant logo

© Copyright 2026, Nutrition Evidence

NED wishes to thank the following organisations for their support:

We use cookies to improve your experience and analyze site traffic with Google Analytics. By continuing to use our site, you agree to our use of cookies. Learn more.