Elias Taylor Durgante Severo, Fred Willians Calonego, Carlos Alberto Oliveira de Matos
Journal: Bioresource technology 2010;101(7):2545-8
PMID: 20007016
The objective of this study was to evaluate the effect of log steaming and of the diametrical position of boards on the timber quality of Eucalyptus grandis. Logs with diameters between 20 and 25 cm, between 25 and 30 cm and between 30 and 35 cm were studied. Half of logs were kept in its original condition, and the other half was steamed at 90 degrees C for 20 h. Later, the logs were cut into flat saw boards, and defects due to growth stress relief were measured. The results show that: (1) boards from control logs show different magnitudes of cracking according to the diameter of the log and the diametrical position of the board; (2) boards from logs with diameters between 30 and 35 cm and those from next to the pith develop larger cracks; and (3) boards from steamed logs show a reduction in the magnitude of cracking and a homogenous distribution of this defect relative to diametrical position within the log.
Copyright 2009 Elsevier Ltd. All rights reserved.
Full Text Sources:
© Copyright 2026, Nutrition Evidence
We use cookies to improve your experience and analyze site traffic with Google Analytics. By continuing to use our site, you agree to our use of cookies. Learn more.